Porous carbon material was synthesized from sugarcane bagasse by 2 steps. Firstly, increase the surface area by treatment bagasse via using hot-compressed with mixture of ethanol/water in various concentrations (0-100%v). Secondly, transform the pretreated bagasse to porous carbon by carbonization under nitrogen at 900°C for 2 hours. The highest surface area was found at a pretreatment temperature 180°C with mixture of ethanol-water 25%v and specific surface area was 382 m2/g while raw bagasse without pretreated was 189 m2/g. Pretreated bagasse and porous carbon were analyzed by Scanning Electron Microscopy (SEM), Fourier Transform Infrared (FT-IR) analysis and surface area measurement by N2 adsorption (BET). The result was showed that organosolv pretreatment using ethanol mixed water can increase the surface area and porosity of bagasse.
Citation
Materials Today Proceedings, 4(5), 6261-6266, 2017