Preparation of BST Powders and Ceramics via a Hybrid Method
| dc.contributor.author | Klaytae, Thanawat | |
| dc.contributor.author | Vittayakorn, Naratip | |
| dc.contributor.author | Sumang, Rattiphorn | |
| dc.date.accessioned | 2026-08-06T10:39:22Z | |
| dc.date.available | 2026-08-06T10:39:22Z | |
| dc.date.issued | 2023-01-01 | |
| dc.description.abstract | Barium strontium titanate (Ba<inf>0.8</inf>Sr<inf>0.2</inf>TiO<inf>3</inf>; BST) ceramics, were prepared by the hybrid method between Solid-state reaction (SSR) and Sol-gel methods (SG) in a ratio of 1:0.1–1:0.5. The BST powder was successfully calcined at 850 °C for 2 h. This temperature is much lower than the calcination temperatures of the SSR method. The BST ceramics were sintered between 1150 and 1450 °C. All samples showed the pure perovskite structure corresponding to JCPDS no. 34-0411. The optimum sintering temperature was observed from the samples sintered at 1450 °C for 4 h, indicating a density of 5.26 g/cm<sup>3</sup>, dielectric constant of 7018, and ferroelectric properties: (P <inf>max</inf> = 13.8 μC/cm<sup>2</sup>, P <inf>r</inf> = 2.5 μC/cm<sup>2</sup> and E <inf>c</inf> = 2.3 kV/cm at 30 kV/cm). | |
| dc.identifier.citation | Integrated Ferroelectrics, 238(1), 224-237, 2023 | |
| dc.identifier.doi | 10.1080/10584587.2023.2234571 | |
| dc.identifier.issn | 10584587 | |
| dc.identifier.other | 2-s2.0-85173545109 | |
| dc.identifier.uri | https://dspace.kmitl.ac.th/handle/123456789/13851 | |
| dc.source | Integrated Ferroelectrics | |
| dc.subject | ferroelectric | |
| dc.subject | hybrid method | |
| dc.subject | microstructure | |
| dc.subject | Phase transition | |
| dc.title | Preparation of BST Powders and Ceramics via a Hybrid Method | |