Preparation of SiO<sub>2</sub>-diamond composites by spark plasma sintering

dc.contributor.authorMettaya Kitiwan
dc.contributor.authorHirokazu Katsui
dc.contributor.authorTakashi Goto
dc.date.accessioned2025-07-21T06:05:28Z
dc.date.issued2021-07-03
dc.description.abstractSiO2-diamond composites with 65–85 mass% diamond were fabricated by spark plasma sintering at 1873 K under 130 MPa for 300 s using bimodal diamond particle size of 2 and 25 µm in diameter. The diamond particles were coated with a SiC layer by chemical vapor deposition. The effects of diamond content on relative density, microstructure, and Vickers hardness of the SiO2-diamond composites were investigated. The SiO2-diamond composites exhibited relative density of 96%, and Vickers hardness of 36.2 ± 3.6 GPa at 75 mass% diamond content.
dc.identifier.doi10.1080/21870764.2021.1952745
dc.identifier.urihttps://dspace.kmitl.ac.th/handle/123456789/10487
dc.subjectSpark Plasma Sintering
dc.subjectVickers hardness test
dc.subjectRelative density
dc.subjectParticle (ecology)
dc.subject.classificationAdvanced materials and composites
dc.titlePreparation of SiO<sub>2</sub>-diamond composites by spark plasma sintering