Characterization of PVA-Chitosan Nanofibers Prepared by Electrospinning

dc.contributor.authorK. Paipitak
dc.contributor.authorT. Pornpra
dc.contributor.authorP. Mongkontalang
dc.contributor.authorW. Techitdheer
dc.contributor.authorW. Pecharapa
dc.date.accessioned2025-07-21T05:51:49Z
dc.date.issued2011-01-01
dc.description.abstractPVA/Chitosan nanocomposite fibers were prepared by electrospinning method. The weight ratio of PVA:Chitosan was fixed at 80:20 in 2% Acetic acid. The concentration of the PVA/Chitosan solution was varied from 3 to 5 wt%. The viscosity of precursor solution was determined by Ubbelohe viscometer. The results revealed that the mixture solution viscosity is directly proportional to its concentration. The morphology and diameter of PVA/Chitosan nanocomposite fibers were characterized by scanning electron microscopy and atomic force microscopy. The diameter of as-prepared PVA/Chitosan nanocomposite fiber was approximately 100 nm. The suitable concentration condition of the solution for fiber formation is 5wt% due to the maximum fiber yield. Fourier Transform Infrared Spectroscopic measurement exhibited the existence of relevant functional groups of both PVA and Chitosan in the composites.
dc.identifier.doi10.1016/j.proeng.2011.03.019
dc.identifier.urihttps://dspace.kmitl.ac.th/handle/123456789/2811
dc.subjectElectrospinning
dc.subject.classificationElectrospun Nanofibers in Biomedical Applications
dc.titleCharacterization of PVA-Chitosan Nanofibers Prepared by Electrospinning
dc.typeArticle