CuBO2 is prepared by a solid-state reaction method to investigate thermoelectric properties in high temperature. The XRD result confirms the CuBO2 compound existing in this method. The Seebeck reveals the compound displays p-type thermoelectric material. The experimental results of electrical resistivity exhibited results of 0.004 S/cm to 0.038 S/cm with the temperature range of 650 to 830 K. The Seebeck value is in the range of 450 μV/K to 950 μV/K, and the thermal conductivity is in the range of 1.4 × 10-5 to 5.3 × 10-5 W/m-K2 with the same temperature. The maximum PF and ZT is 5.3 × 10-5 W/m-K2 and 0.0016, respectively, at 960 K. This work demonstrates that the CuBO2 delafossite-oxide compound displays the p-type thermoelectric materials. © 2014 IEEE.

Description

Keywords

Delafossite, Solid state, Thermoelectric

Citation

Jictee 2014 4th Joint International Conference on Information and Communication Technology Electronic and Electrical Engineering, 2014

Collections

Endorsement

Review

Supplemented By

Referenced By