  4. Characterization of PVA-chitosan nanofibers prepared by electrospinning
Loading...
Thumbnail Image

Characterization of PVA-chitosan nanofibers prepared by electrospinning

Author(s)
Paipitak, K.
Pornpra, T.
Mongkontalang, P.
Techitdheer, W.
Pecharapa, W.
Date Issued
May 2, 2011
Type
Conference Paper
DOI
10.1016/j.proeng.2011.03.019
Abstract
PVA/Chitosan nanocomposite fibers were prepared by electrospinning method. The weight ratio of PVA:Chitosan was fixed at 80:20 in 2% Acetic acid. The concentration of the PVA/Chitosan solution was varied from 3 to 5 wt%. The viscosity of precursor solution was determined by Ubbelohe viscometer. The results revealed that the mixture solution viscosity is directly proportional to its concentration. The morphology and diameter of PVA/Chitosan nanocomposite fibers were characterized by scanning electron microscopy and atomic force microscopy. The diameter of as-prepared PVA/Chitosan nanocomposite fiber was approximately 100 nm. The suitable concentration condition of the solution for fiber formation is 5wt% due to the maximum fiber yield. Fourier Transform Infrared Spectroscopic measurement exhibited the existence of relevant functional groups of both PVA and Chitosan in the composites.
Citation
Procedia Engineering, 8, 101-105, 2011
Subjects

Chitosan

Electrospinning

Nanofibers

PVA

Metrics
Get Involved!
  • Source Code
  • Documentation
  • Slack Channel
Make it your own

DSpace-CRIS can be extensively configured to meet your needs. Decide which information need to be collected and available with fine-grained security. Start updating the theme to match your Institution's web identity.

Need professional help?

The original creators of DSpace-CRIS at 4Science can take your project to the next level, get in touch!

Built with DSpace-CRIS software - Extension maintained and optimized by 4Science

  • Accessibility settings
  • Privacy policy
  • End User Agreement
  • Send Feedback