    Preparation of lead zirconate-lead nickel niobate ceramics by the reaction sintering process
    (2009-12-01) ; ;
    Niemcharoen, Surasak
    ;
    ;
    Laoratanakul, Pitak
    The perovskite structure of lead zirconate - lead nickel niobate ceramics, (1-x) PbZrO3-xPb(Ni1/3Nb2/3)O3 (PZ - PNN) at x between 0.00-0.50, has been prepared by the reaction-sintering process. The specimens were prepared directly from a mixture of their constituent oxide without any calcination step. The PZ - PNN ceramics could be obtained after 6 h sintering at 1,100-1,250°C. Crystal structure and phase transition of PZ-PNN were investigated by x-ray diffraction (XRD). XRD indicated that the structure of PZ-PNN ceramics is orthorhombic for a composition where x = 0.00, rhombohedral for compositions where x = 0.10 ≤ x ≤ 0.40 and pseudo-cubic for a composition where x = 0.50. The dielectric properties of the ceramics were measured as functions of both temperature and frequency. The results indicated that the transition temperature decreases with increasing PNN concentration. Furthermore, morphology and grain size evolution have been determined via a scanning electron microscope (SEM). Copyright © Taylor & Francis Group, LLC.
  • Some of the metrics are blocked by your 
    Item type:Publication,
    The phase evolution with temperature in 0.94PbZrO3-0. 06Pb(Mg1/2W1/2)O3 antiferroelectric ceramic
    (2010-09-10)
    Charoonsuk, Piyanut
    ;
    ; ;
    Niemcharoen, Surasak
    ;
    The perovskite structure of the lead zirconate-lead magnesium tungstate ceramic, 0.94PbZrO<inf>3</inf>-0.06Pb(Mg<inf>1/2</inf>W<inf>1/2</inf>)O <inf>3</inf> (0.94PZ-0.06PMW), was prepared by the wolframite precursor method. The phase evolution with temperature in the 0.94PZ-0.06PMW ceramic was investigated, with dielectric permittivity, differential scanning calorimetry and polarization measurements. The ceramic was in the antiferroelectric phase when below 177 °C, based on dielectric measurement, and an intermediate phase was detected between 177 and 219 °C. Evidence from ferroelectric data was found to suggest that this intermediate phase is ferroelectric. © 2010 Elsevier B.V. All rights reserved.